SuperDuplex stainless like Duplex, is a mixed microstructure of austenite and ferrite (50/50) which has improved strength over ferritic and austenitic steel grades. The main difference is that Superduplex has a higher Molybdenum and Chromium content which gives the material greater corrosion resistance.
SuperDuplex has the same benefits as its counterpart – it has lower production costs when compared with similar ferritic and austenitic grades and due to the materials increased tensile and yield strength, in many cases this gives the purchaser the welcomed option of purchasing smaller thicknesses without the need to compromise on quality and performance.
SuperDuplex is used in the oil and gas industry, on offshore platforms, in heat exchangers, chemical processing equipment pressure vessels and boilers.
2507 is the most common Super Duplex alloy which contains 24% chromium and a minimum of 3% molybdenum. Please refer to the chemical composition and mechanic properties tables below. For information on Duplex alloy please click here.
UNS No | S32750 |
---|---|
EN | 1.441 |
AISI | 2507 |
Carbon (C) | 0.03 |
Silicon (Si) | 0.8 |
Manganese (Mn) | 1.2 |
Phosphorus (P) | 0.035 |
Sulphur (S) | 0.02 |
Chromium (Cr) | 24.0/26.0 |
Molybdenum (Mo) | 3.0/3.5 |
Nickel (Ni) | 6.00/8.00 |
Nitrogen (N) | 0.24/0.32 |
Other | Cu: 0.50 |
DESCRIPTION | DUPLEX 2205 |
---|---|
Proof Stress 0.2% (MPa) | 450 |
Tensile strength (MPa) | 620 |
Elongation A5 (%) | 20 |
Hardness | HB: 293 HRB: 96 (according to Rockwell C Scale) |
Density | lb/in3 | 0.28 |
---|---|---|
Modulus of Elasticity | psi x 106 | 29 |
Coefficient of Thermal Expansion 68-212°F/°F | x10-6/°F | 7.2 |
Thermal Conductivity | Btu/h ft °F | 8.7 |
Heat Capacity | Btu/lb/°F | 0.12 |
Electrical Resistivity | W-in x 10-6 | 31.5 |
ASTM/ASME ………. A240 – UNS S32750
EURONORM………… 1.4410 – X2 Cr Ni MoN 25.7.4
AFNOR……………….. Z3 CN 25.06 Az